DNMG110408 DNMG332 PM Cnc Turning Blade Carbide Inserts YBC152 for Steel DNMG110404
Advantages:
Specification:
Brand | Speed |
Model | DNMG110408/110404 |
Color | yellow, copper, black, blue color and colorful coating |
Workpiece | Steel, stainless steel, cast iron, Aluminum and etc., |
Type | Turning Tools |
Package | 10pcs/box |
Coating | pvd and cvd |
Weight | 0.015kg |
Usage | External Turning tools |
Hardness | 20-65HRC |
Material | Tungsten Cardide Inserts |
Processing Type | Medium Cutting |
Application:
Our DNMG tungsten carbide Turning Inserts is made of imported base material with advanced high precision, which enhances the quality of the blade, high hardness, good ductility, high finish, thick coating, stable performance and improves the processing efficiency. The unique coating process, fine and smooth, no drip marks, reduce surface friction, so that the cutting resistance is smaller. The high heat resistance and cobalt rich gradient structure cemented carbide matrix makes DNMG tungsten carbide inserts have a series of excellent properties such as high hardness, wear resistance, good strength and toughness. The DNMG blades are sintered at 5000 ℃ to remove impurities, and sprayed by 1000 ℃ stress accumulation. The unique coating process makes the processing more stable, smooth cutting, good chip removal performance, not easy to produce chip buildup, and the processing surface has good smoothnes. And the carbide inserts are sharp and thick, so that the cutting speed is fast but not easy to break. It has wide range of application, applicable to step surface processing, model profiling processing, grooving cutting, slope processing, and could to be processed alloy steel, soft steel, carbon steel, medium steel, stainless steel, cast iron, titanium alloy,
please send me your requirements to us, we will recommend the best suitable grade.
Products Detail:
Details:
1. Our perfect edge treatments, every pieces can stand the test.
2. Longer tools service life improve your working efficiency.
Note:
1. Carbide turning inserts shall not be bumped or dropped on the ground and please be handled with care.
2. Before installing the carbide turning blade, please confirm the performance and use of operation table, and the cutting direction indicated by the arrow of the blade is consistent with the rotation direction of the operation table. Please pay attention to don't install in the opposite direction. The wrong installation direction may cause the blade serrations to fall off, in case of accidents.
3. After installation, it is necessary to confirm whether the center hole of the carbide blade is firmly fixed on the flange of the saw table. If necessary, put on a spacer, then, push it lightly by hand to confirm whether the blade rotates eccentrically.
4. When using, do not exceed the specified high speed.
5. When not using, please hang the blades upright on a dry rack.
FAQ:
1. Flank wear: (This is a common form of failure)
Effect: Gradual change in workpiece size or loss of surface finish
Reason: Linear speed is too high, and reach to service life of the tool
Measures: Adjust the processing parameters, such as reducing the linear speed and changing to inserts with higher wear resistance
2.Breakdown problem: (bad form of failure)
Effects: Sudden changes in workpiece size or surface finish, causes sparks and surface burrs
Reason: Inappropriate setting of processing parameters, inappropriate selection of blade material, poor workpiece rigidity, or unstable blade clamping
Measures: Check whether the parameter settings are reasonable, and select the corresponding tool according to the workpiece
3. Severely broken: (a very bad form of failure)
Effect: sudden and unpredictable occurrence, resulting in scrapped tool holder material or defective workpiece and scrapped
Reason: The processing parameters are set incorrectly, the vibration tool workpiece or the insert is not installed in place
Measures: Set reasonable processing parameters. The feed rate and cutting should be reduced, the corresponding machining insert should be selected, and the rigidity of the workpiece and insert should be strengthened.
4. Built-up edge:
Effects: Inconsistent workpiece dimensions and poor surface finish. Fluff or burrs adhere to the workpiece surface
Reason: The cutting speed is too low, the feed is too low, and the blade is not sharp enough
Measures: Increase the cutting speed and use a sharper insert for the feed
CONTACT US AT ANY TIME