MGMN250-G MGMN300 MGMN400 MGMN500 M Cut-off Cnc Grooving Insert PVD and CVD Coating Lathe Tools
Advantages:
Specification:
Brand | Speed |
Model | MGMN150/200/250/300/400/500 |
Color | yellow, copper, black |
Workpiece | Steel, stainless steel, cast iron, etc |
Customized | OEM, ODM |
Package | plastic boxes |
Coating | pvd, cvd |
Weight | 15g |
Usage | External Turning tool |
Hardness | 20-65HRC |
Material | Tungsten Cardide |
Processing Type | Cnc Cutting |
Application:
Our MGMN tungsten carbide grooving inserts adopts imported Dorst machine to ensure good stability of cutting edge, high precision, high hardness, good finishing, durable coating, stable performance and improves the working efficiency. MGMN carbide groove insert is made of imported base material with advanced high precision, which enhances the quality of the blade, high hardness, good ductility, high finish, thick coating, stable performance and improves the processing efficiency; Unique coating process, fine and smooth, no drip marks, reduce surface friction, so that the cutting resistance is smaller; High precision blade, effectively reducing friction and loss; The blade is sharp and thick, so that the cutting speed is fast but not easy to break. It has wide range of application, applicable to step surface processing, model profiling processing, grooving cutting, slope processing, and could to be processed alloy steel, soft steel, carbon steel, medium steel, stainless steel,cast iron, titanium alloy, etc.,
please send me your requirements to us, we will recommend the best suitable grade.
Products Detail:
G: Mainly used for cutting off, the special chipbreaker groove design narrows the cutting
M: It can meet various processing needs such as cutting, grooving and turning, finishing and rough machining are available, and smooth chip removal
T: Semi-finishing groove for medium cuts
Details:
1. Our perfect edge treatment, every piece can stand the test.
2. Longer tools service life improve your working efficiency.
Company Profile
Hunan SPEED Carbide Tools Co.,Ltd is a professional supplier of Carbide, Inserts,Including Turning Inserts,Milling Inserts,Grooving Inserts,Threading Inserts,U drill lnserts, Aluminum Inserts and Cermet inserts etc. Located in ZhuzhouHunan, which is the biggest tungsten carbide tools city near ZCCCT, We provide various and efficient delivery ways. Our factory covers and area of 2,000sqm and has more than 100 staff members who are professional and willing to grow up with you.
Below is our factory and warehouse, we use
1. 100% virgin raw material + Germany machine DORST make perfect quality
2. each piece of insert have 3 times checked before shipment.
Feel free to contact if you want a factory show.
Note:
1. Carbide grooving inserts shall not be bumped or dropped on the ground and please be handled with care.
2. Before installing the carbide grooving blade, please confirm the performance and use of operation table, and the cutting direction indicated by the arrow of the blade is consistent with the rotation direction of the operation table. Please pay attention to don't install in the opposite direction. The wrong installation direction may cause the blade serrations to fall off, in case of accidents.
3. After installation, it is necessary to confirm whether the center hole of the carbide grooving blade is firmly fixed on the flange of the saw table. If necessary, put on a spacer, then, push it lightly by hand to confirm whether the blade rotates eccentrically.
4. When using, do not exceed the specified high speed.
5. When not using, please hang the blades upright on a dry rack.
FAQ:
1. Flank wear: (This is a common form of failure)
Effect: Gradual change in workpiece size into a decrease in surface finish
Reason: the line speed is too high, and the service life of the tool is reached
Measures: Adjust the processing parameters, such as reducing the line speed and changing to inserts with higher wear resistance
⒉Breakdown problem: (bad form of failure)
Effects: Sudden changes in workpiece size or surface finish, resulting in sparking surface burrs
Reason: Inappropriate setting of processing parameters, inappropriate selection of blade material, poor workpiece rigidity, unstable blade clamping
Measures: Check whether the parameter settings are reasonable, and select the corresponding tool according to the workpiece
3. Severely broken: (a very bad form of failure)
Effect: sudden and unpredictable occurrence, resulting in scrapped tool holder material or defective workpiece and scrapped
Reason: The processing parameters are set incorrectly, the vibration tool workpiece or the blade is not installed in place
Measures: Set reasonable processing parameters. The feed rate and cutting should be reduced, the corresponding machining insert should be selected, and the rigidity of the workpiece and insert should be strengthened.
4. Built-up edge:
Effects: Inconsistent workpiece dimensions and poor surface finish. Fluff or burrs adhere to the workpiece surface
Reason: The cutting speed is too low, the feed is too low, the blade is not sharp enough
Measures: Increase the cutting speed and use a sharper insert for the feed