Carbide Drilling Inserts Cnc U drill WC Style WCMX080412-FN for Steel, Stainless Steel
Advantages:
Specification:
Brand | Speed |
Model | WCMX030208, WCMX040208, WCMX050308, WCMX06T308, WCMX080412 |
Color | yellow, copper, black, nano blue, colorful coating |
Workpiece | Steel, stainless steel, cast iron, Aluminum |
Type | Drilling Tools |
Package | 10pcs/box |
Coating | pvd & cvd |
Weight | 0.015kg |
Usage | External Turning tools |
Hardness | 20-65HRC |
Material | Tungsten Cardide Inserts |
Processing Type | Medium Cutting |
Application:
Our WC type tungsten carbide drilling inserts is made of imported base material with advanced high precision, which enhances the quality of the inserts, high hardness, good ductility, high finish, thick coating, stable performance and improves the processing efficiency. And we adopts imported machine to ensure good stability of cutting edge, high precision. The unique coating process, fine and smooth, no drip marks, reduce surface friction, so that the cutting resistance is smaller. And the carbide inserts are sharp and thick, so that the cutting speed is fast but not easy to break. It has wide range of application, applicable to step surface processing, model profiling processing, grooving cutting, slope processing, and could to be processed alloy steel, soft steel, carbon steel, medium steel, stainless steel, cast iron, titanium alloy,
please send me your requirements to us, we will recommend the best suitable grade.
Products Detail:
Details:
1. Below is our perfect edge treatments, every pieces can stand the test.
2. The Longer tools service life improving your working efficiency.
FAQ:
1. Flank wear: (Common problem)
Effect: Gradual change in workpiece size or loss of surface finish
Reason: Linear speed is too high, and reach to service life of the tool
Measures: Adjust the processing parameters, such as reducing the linear speed and changing to inserts with higher wear resistance
2.Breakdown problem:
Effects: Sudden changes in workpiece size or surface finish, causes sparks and surface burrs
Reason: Inappropriate setting of processing parameters, inappropriate selection of blade material, poor workpiece rigidity, or unstable blade clamping
Measures: Check whether the parameter settings are reasonable, and select the corresponding tool according to the workpiece
3. Severely broken: (bad situation)
Effect: sudden and unpredictable occurrence, resulting in scrapped tool holder material or defective workpiece and scrapped
Reason: The processing parameters are set incorrectly, the vibration tool workpiece or the insert is not installed in place
Measures: Set reasonable processing parameters. The feed rate and cutting should be reduced, the corresponding machining insert should be selected, and the rigidity of the workpiece and insert should be strengthened.
4. Built-up edge:
Effects: Inconsistent workpiece dimensions and poor surface finish. Fluff or burrs adhere to the workpiece surface
Reason: The cutting speed is too low, the feed is too low, and the blade is not sharp enough
Measures: Increase the cutting speed and use a sharper insert for the feed